Cyro Acrifix® 117 Acrylic Cement
Subcategory: Vinyl; Acrylic; Thermoplastic
Material Notes: ACRIFIX 117 solvent acrylic cement is a clear, fluid adhesive free of dichloromethane (methylene chloride). Dichloromethane is currently listed as a suspected carcinogen by the EPA, IARC and ACGIH. With that in mind, ACRIFIX 117 solvent cement was developed utilizing a patented formula to provide an alternative to cements containing dichloromethane. With regard to performance, ACRIFIX 117 solvent cement can be used to bond ACRYLITE PLUS® acrylic sheet, ACRYLITE® FF acrylic sheet and ACRYLITE® GP acrylic sheet to themselves and to each other. ACRIFIX 117 cement does not cause crazing or blushing (whitening) when used as recommended under normal conditions. Also, the bonds produced from ACRIFIX 117 cement are strong and clear.Information provided by Cyro Industries
| Available Properties |
- Density
- Solids Content
- Viscosity
- Storage Temperature
- Flash Point
- Refractive Index
- Shelf Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|