Cyro Cyrex® 300 Acrylic-Polycarbonate Alloy

 

Subcategory: Polycarbonate; Acrylic; Thermoplastic

Material Notes:
CYREX 300 alloy is suitable for applications where a high degree of heat resistance is necessary. It has a deflection temperature of 253°F and a Vicat softening point of 306°F whereas CYREX 200 alloy has a deflection temperature of 214°F and a Vicat softening point of 277°F.

Information provided by Cyro Industries

Available Properties
  • Specific Gravity
  • Water Absorption
  • Linear Mold Shrinkage
  • Melt Flow
  • Hardness, Rockwell M
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Notched
  • CTE, linear, 212°F (100°C)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • Flammability, UL94
  • Chemical Resistance to Acetone
  • Chemical Resistance to Ammonia
  • Chemical Resistance to Antifreeze
  • Chemical Resistance to Baking Soda Paste
  • Chemical Resistance to Bleach 10%
  • Chemical Resistance to Butter
  • Chemical Resistance to Citric Acid Solution (0.1%)
  • Chemical Resistance to Coffee
  • Chemical Resistance to Diesel Fuel
  • Chemical Resistance to DOP (Phthalate)
  • Chemical Resistance to Ethanol
  • Chemical Resistance to Ethylene Glycol
  • Chemical Resistance to Fantastic Cleaner
  • Chemical Resistance to Fluorides
  • Chemical Resistance to Frenchs Mustard
  • Chemical Resistance to Gasoline
  • Chemical Resistance to Glycerin
  • Chemical Resistance to Heavy Duty Detergent
  • Chemical Resistance to Heptane
  • Chemical Resistance to Igepal (1%) Solution
  • Chemical Resistance to IPA
  • Chemical Resistance to IPA/Water 50%
  • Chemical Resistance to Kerosene
  • Chemical Resistance to Lipids
  • Chemical Resistance to Lipstick
  • Chemical Resistance to Octane/Toluene 75%/25%
  • Chemical Resistance to Rust Inhibitor Veto #4224
  • Chemical Resistance to Rust Inhibitor Veto #53359
  • Chemical Resistance to Soap and Water
  • Chemical Resistance to Sodium Hydroxide (0.5%)
  • Chemical Resistance to Tea
  • Chemical Resistance to Toothpaste
  • Chemical Resistance to Transmission Fluid
  • Chemical Resistance to Vinyl Gasket
  • Resistance to Palmolive Dishwasher/Water 50%
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。