Cyro XT® 375TE Acrylic Based Multipolymer Compound
Subcategory: Acrylic; Thermoplastic
Material Notes: XT® polymer 375TE acrylic-based multipolymer compound is a tough, transparent, tamper-evident medical packaging material that will stress whiten if punctured. The tamper-evident, stress whitening characteristic allows for easier inspection to determine if the integrity of the packaging has been compromised. Additionally, the color tint of the transparent material allows for an easy visual inspection of the seal between the lidding stock and the package.Information provided by Cyro Industries
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell M
- Tensile Strength, Yield
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Tensile Modulus
- Flexural Modulus
- Flexural Modulus
- Flexural Strength
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched
- CTE, linear, 212°F (100°C)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Refractive Index
- Haze
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|