Cyro MMA Methyl Methacrylate Monomer, Inhibited
Subcategory: Methacrylate; Thermoplastic
Material Notes: Monomeric methyl methacrylate is one of the more important esters of methacrylic acid. It`s clear, colorless, volatile liquid with a characteristic odor. MMA is slightly soluble in water and miscible with most organic solvents.Information provided by Cyro Industries
| Available Properties |
- Density
- Specific Gravity
- Solubility of Water
- Solubility in Water
- Viscosity
- Molecular Weight
- Vapor Pressure
- Specific Heat Capacity
- Boiling Point
- Heat of Formation
- Flash Point
- Refractive Index
- Melt Temperature
- Explosive Limits, vol. % in air
|
|
|
|