Cyro Vu-Stat™ C37 Static Dissipative Acrylic Multipolymer Compound
Subcategory: Acrylic; Thermoplastic
Material Notes: Vu-Stat C-37 compound is a transparent, electro-static dissipative acrylic multipolymer compound with outstanding ESD properties and an excellent balance of mechanical, thermal and flow properties. Developed specifically for electronic parts that are sensitive to static discharge, Vu-Stat C-37 compound retains permanent static dissipative properties even after several washings. This product can be processed in all types of injection molding presses.Information provided by Cyro Industries
| Available Properties |
- Melt Flow
- Hardness, Rockwell L
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Static Decay
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Haze
- Gloss
- Transmission, Visible
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Injection Pressure
- Back Pressure
- Screw Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|