Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply
Subcategory: Epoxy; Thermoset
Material Notes: CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue life in conventional reinforced plastics. CYPLY® 1002 uses type E continuous filament fiberglass. It is supplied as cured panels or cut to size shapes. CYPLY 1002 is available in unidirectional, crossply, or isotropic fiber orientation, each offering a different balance of properties. Features and benefits include: - High impact strength
- chemical and corrosion resistance
- high strength-to-weight ratio
- excellent fatigue life and high strain capability
- low notch sensitivity
- increased design options (springs to rail joints)
- resistant to solvents and cleaning fluids
- less downtime in harsh environments
- weight reduction
- greater capacity to store energy than 1060 spring steel
Information provided by Red Seal Electric Company.
| Available Properties |
- Specific Gravity
- Filler Content
- Hardness, Barcol
- Tensile Strength, Ultimate
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Shear Modulus
- Volume Resistivity
- Insulation Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- CTE, linear 68°F
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|