Daikin DAI-EL G-575 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 70% Fluorine Content
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Material Notes: Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application. Features: Low permeability to gasoline and alcohol mixed fuel oil and good extrudability. Information provided by Daikin Industries.
| Available Properties |
- Specific Gravity
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Tear Strength
- Compression Set
- Compression Set, Elevated Temperature
- Minimum Service Temperature, Air
- Brittleness Temperature
- Processing Temperature
- Cure Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|