Daikin DAI-EL G-501NK Fluoroelastomer Terpolymer, Diamine Curable Grade, 68% Fluorine Content
Subcategory: Fluoropolymer, TS; Elastomer, TPE; Thermoset
Material Notes:
Features: Good mechanical characteristics. Information provided by Daikin Industries.
| Available Properties |
- Specific Gravity
- Oxygen Transmission
- Nitrogen Transmission
- Carbon Dioxide Transmission
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Tear Strength
- Compression Set
- Compression Set, Elevated Temperature
- Minimum Service Temperature, Air
- Brittleness Temperature
- Processing Temperature
- Cure Time
|
|
|
|