Daikin ACX-34 NEOFLON PFA Coating Powder, White
Subcategory: Fluoropolymer; Thermoplastic; PFA
Material Notes: NEOFLON PFA coating powder is designed for high build coatings having excellent resistance to chemical and corrosive environments. Description: 30-80 micron thickness. Processing Methods: Electrostatic spray coating. Information provided by Daikin Industries.