Daikin EA-LR43 NEOFLON ETFE Pellets
Subcategory: Fluoropolymer; Thermoplastic; ETFE/ECTFE
Material Notes: Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, flaring post-forming processes, and others. Applications:Bonding material for multilayer coextrusion of Nylon 12 and EP-600 series resin. Information provided by Daikin Industries.
| Available Properties |
- Specific Gravity
- Bulk Density
- Water Absorption
- Oxygen Transmission
- Nitrogen Transmission
- Viscosity
- Linear Mold Shrinkage
- Melt Flow
- Deformation
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Compressive Strength
- Izod Impact, Unnotched
- Coefficient of Friction
- Coefficient of Friction, Static
- Taber Abrasion, mg/1000 Cycles
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Flammability, UL94
- Oxygen Index
- Chemical Resistance
- Contact Angle
- Weatherability
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|