Nitriflex N-726 NBR - Nitrile Rubber
Subcategory: Elastomer, TS; Thermoset
Material Notes: Ideal for applications that require good performance at low temperatures and moderate resistance to oils. Applications: fuel hose packing, gaskets, diaphragms, print rolls. Information provided by Dax Resinas
| Available Properties |
- Volatiles
- Mooney Viscosity
- Ash
- Appearance
- Bound Acrylonitrile Content (%)
- Polymerization
|
|
|
|