Nitriflex SB-1009 Styrene Butadiene Copolymer
Subcategory: Styrene-Butadiene; Thermoplastic
Material Notes:
Applications: Used to promote better dimensional stability in articles like profiles, hoses, shoe sole and also recommended to PSA adhesives and adhesives for vertical applications. Available in bale and granules (G). Information provided by Dax Resinas
| Available Properties |
- Volatiles
- Mooney Viscosity
- Linear Mold Shrinkage
- Ash
- Styrene Content
- Appearance
|
|
|
|