Nitriflex Nitrigum 50 F Styrene Butadiene Rubber
Subcategory: Styrene-Butadiene; Elastomer, TS; Thermoset
Close Analogs: FDA-21-CRF172.615 E FCC-V
Material Notes: Food grade polymer. Fully compatible with resins and paraffins, normally used in gum bases. Due to the characteristics of film elasticity, its excellent to bubble gums. Applications: Information provided by Dax Resinas
| Available Properties |
- Volatiles
- Mooney Viscosity
- Ash
- Styrene Content
- Appearance
- BHT (%)
- Residual Styrene (ppm)
|
|
|
|