Nitriflex Nitrimpact 1300 MBS Modifier
Subcategory: Methacrylate; Styrene-Butadiene; Additive/Filler for Polymer
Material Notes: NITRIMPACT™ 1300 thermoplastic resin is a methyl methacrylate-butadiene-styrene (MBS) impact modifier for transparent and opaque PVC applications. Applications: Transparent PVC Compounds (no use restriction for translucents and opaques compounds). Used for blow moulding, extrusion, calandering, thermoforming and injection processes, for the production of artifacts like: transparent profiles, laminates in general, blister packs, tubes, hoses, automotive parts, etc. Information provided by Dax Resinas
| Available Properties |
- Volatiles
- Izod Impact, Notched
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|