Petroquimica Triunfo Trithene® CX 7065 LDPE - Extrusion Coating
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: FDA: 21 CFR 177.1520 (C) 2.1
Material Notes: The Trithene® CX 7065 resin is a product developed especially to meet the segment of extrusion coating where the following properties are necessary: processing stability at high production rates, adhesiveness to various types of substrates, low neck-in, and good optical properties, mainly gloss. Trithene® CX 7065 resin provides its substrates with an excellent barrier against humidity. This product complies with ASTM D1248-IA3.Applications: Extrusion coating of paper and cardboard. Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR. Information provided by Dax Resinas
| Available Properties |
- Density
- Water Vapor Transmission
- Oxygen Transmission Rate
- Thickness
- Melt Index of Compound
- Tensile Strength at Break
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Tensile Strength, Yield
- Elongation at Break
- Secant Modulus, MD
- Secant Modulus, TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop Test
- Melting Point
- Vicat Softening Point
- Haze
- Gloss
- Processing Temperature
- Feed Temperature
- Adapter Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|