Petroquimica Triunfo Trithene® TS 7028 LDPE - Automatic Packaging
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: FDA: 21 CFR 177.1520 (C) 2.1
Material Notes: The Trithene TS 7028 resin is a low-density polyethylene (LDPE) with excellent optical and processability properties that allows for the production of films combining appearance, mechanical strength, and welding along with a uniform thickness. The incorporated additive package confers thermal stability and appropriate coefficient of friction (COF) that are fundamental for achieving high productivity on printing, cutting, welding and bagging lines. This product complies with ASTM standard D1248-IA3 and the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff.Applications: Films for automatic or semi-automatic packaging of food products (grains, powder, or farinaceous) such as cereals, sugar, salt, and flours. Structure-laminated technical films with PP, BOPP, polyester and/or aluminum foil for packaging miscellaneous products such as coffee, crackers, etc. Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR. Information provided by Dax Resinas
| Available Properties |
- Density
- Thickness
- Melt Index of Compound
- Tensile Strength at Break
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Tensile Strength, Yield
- Elongation at Break
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop Test
- Vicat Softening Point
- Haze
- Gloss
- Processing Temperature
- Feed Temperature
- Adapter Temperature
- Blow-up Ratio (BUR)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|