Petroquimica Triunfo Trithene® TU 3001 LDPE - Agricultural Film
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Material Notes: The Trithene TU 3001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical properties, good processability and bubble stability. These qualities ensure the production of very wide films with uniform thickness and excellent resistance to UV-radiation. The additive package warrants thermal and light stabilization for greenhouse mid-life films with very good resistance to the traditional soil disinfecting and crop protection chemicals normally applied in agriculture. This product complies with ASTM standard D1248-IA5.Applications: Films for covering of greenhouses and both large and small tunnels. Films for applications that require high mechanical strength and high resistance to aging from solar radiation (UV radiation exposure). Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR. Information provided by Dax Resinas
| Available Properties |
- Density
- Thickness
- Melt Index of Compound
- Tensile Strength at Break
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Tensile Strength, Yield
- Elongation at Break
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop Test
- Vicat Softening Point
- Haze
- Gloss
- Processing Temperature
- Feed Temperature
- Adapter Temperature
- Blow-up Ratio (BUR)
- UV Stabalizer ppm
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|