Petroquimica Triunfo Trithene® TX 3003 LDPE - Shrink Wrap Film
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: FDA: 21 CFR 177.1520 (C) 2.1
Material Notes: The Trithene® TX 3003 resin is a low-density polyethylene (LDPE) with high molecular weight, presenting excellent mechanical properties. The product provided elevated gloss and transparency, adding value to the printing and finish of the films. Its superior density in comparison to conventional LDPE allows the production of flasks with a greater stiffness and better resistance to the temperatures applied in sterilization processes in autoclaves. Because of its narrow molecular weight distribution and its branched structure, the Trithene® TX 3003 resin provides excellent processability with conventional extruders for LDPE, offers a low consumption of energy during processing, and allows the production of films and flasks with a good dimensional uniformity and excellent surface finish. This product complies with ASTM standard D1248-IIA5 and the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff. Applications: Shrink wrap films for the unitization of bottles of soft drinks, beer, and other beverages, vegetable oils, and hygiene and cleaning products. Bags with a high resistance for animal feed. Flexible flasks with a greater stiffness and better surface finish. Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR. Information provided by Dax Resinas
| Available Properties |
- Density
- Thickness
- Melt Index of Compound
- Tensile Strength at Break
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Tensile Strength, Yield
- Elongation at Break
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop Test
- Vicat Softening Point
- Haze
- Gloss
- Processing Temperature
- Feed Temperature
- Adapter Temperature
- Blow-up Ratio (BUR)
- Die Gap mm
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|