Petroquimica Triunfo Trithene® TX 8079 LDPE - Thermal Shrink Film
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: FDA: 21 CFR 177.1520 (C) 2.1
Material Notes: The Trithene TX 8079 resin is a low-density polyethylene (LDPE) with a high molecular weight that presents an elevated mechanical resistance, which are indispensable characteristics for the operations of unitization of various products such as paints, soft drinks, ceramic materials, palletized products, etc. This resin may be easily processed, making it possible to produce films with good thickness uniformity and shrinking qualities, allowing an adequate unitization that is exempt of breaks. This product complies with ASTM standard D1248-IA5 and the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff.Applications: Shrink wrap films for the unitization and palletizing of various products. Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR. Information provided by Dax Resinas
| Available Properties |
- Density
- Thickness
- Melt Index of Compound
- Tensile Strength at Break
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Tensile Strength, Yield
- Elongation at Break
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop Test
- Vicat Softening Point
- Processing Temperature
- Feed Temperature
- Adapter Temperature
- Blow-up Ratio (BUR)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|