Petroquimica Triunfo Trithene® TX 4003 LDPE and LLDPE Blend - High Resistance Film

 

Subcategory: Polyethylene; Thermoplastic; LLDPE; LDPE; Polymer

Key Words: FDA: 21 CFR 177.1520 (C) 2.1

Material Notes:
The Trithene® TX 4003 resin is a blend of low-density polyethylene (LDPE) of high molecular weight with linear low-density polyethylene (LLDPE) designed for the production of industrial films. Since it presents gains in resistance in the weld region, this product meets the requirements of the cutting and welding line and/or of the automatic or semi-automatic packaging, contributing to the reduction of losses due to sacks breaking. The Trithene® TX 4003 resin presents excellent performance on conventional extruders for LDPE, ensuring thermal stability during the processing and allowing the production of films with good thickness uniformity. The components that form the product Trithene® TX 4003 complies with the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff.

Applications: Technical films for high resistance industrial packages and plastic tarps for various uses such as for covering structures and sheds, films for waterproofing, etc. Industrial bags, bags for packaging with greater mechanical resistance as well as against perforation and impact.

Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.

Information provided by Dax Resinas

Available Properties
  • Density
  • Thickness
  • Melt Index of Compound
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Secant Modulus, MD
  • Secant Modulus, TD
  • Coefficient of Friction
  • Elmendorf Tear Strength, MD
  • Elmendorf Tear Strength, TD
  • Dart Drop Test
  • Haze
  • Gloss
  • Processing Temperature
  • Feed Temperature
  • Adapter Temperature
  • Blow-up Ratio (BUR)
  • Die Gap mm
  • Proportion LLDPE %
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。