Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8 and LDPE Blend
Subcategory: Polyethylene; Thermoplastic; LLDPE; LDPE; Polymer
Key Words: FDA: 21 CFR 177.1520 (C) 2.1
Material Notes: The Trilene® TS 8056 product is a blend with a high ratio of linear low-density polyethylene - octene comonomer (LLDPE-C8) with low-density polyethylene (LDPE) with elevated processability, ensuring the production of films with uniform thickness and good visual appearance and weldability. This product presents excellent puncture resistance, exactly to the low temperatures, what it becomes it especially adequate the production of packings for frozen products, as cuts of meat and chicken with or without bone, fish, seafood and ice. The additive package gives it thermal stability, low blocking, and adequate slip performance, which are indispensable to allow high productivity on the extrusion, printing, and finishing lines. The resin should be processed in extruders that are designed or adapted for LLDPE. The components that form the product Trilene® TS 8056 complies with the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff.Applications: Technical laminated films designed for packaging of various products such as coffee, crackers, etc. Technical films for automatic or semi-automatic packaging of solid products (grains, powdered, etc.), liquids (milk, yogurt, etc.), and frozen foods (poultry, beef cuts, seafood, ice, etc.). Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR. Information provided by Dax Resinas
| Available Properties |
- Density
- Thickness
- Melt Index of Compound
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop Test
- Haze
- Gloss
- Processing Temperature
- Feed Temperature
- Adapter Temperature
- Die Cooling Temperature
- Blow-up Ratio (BUR)
- Die Gap mm
- Proportion LLDPE %
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|