Petroquimica Triunfo Trilene® TS 8058 LLDPE-C6 and LDPE Blend

 

Subcategory: Polyethylene; Thermoplastic; LLDPE; LDPE

Key Words: FDA: 21 CFR 177.1520 (C) 2.1

Material Notes:
The Trilene® TS 8058 product is a blend with a high ratio of linear low-density polyethylene - hexene comonomer (LLDPE-C6) with low-density polyethylene (LDPE) excellent mechanical resistance, along with good optical properties and weldability. This product presents good processability with design extruders or adapted for the processing of LLDPE, allowing for the production of films with uniform thickness and good visual appearance. The additive package gives it thermal stability, low blocking and adequate slip performance, which are indispensable to allow high productivity on the extrusion, printing, and finishing lines. The components that form the product Trilene® TS 8058 complies with the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff.

Applications: Technical laminated films designed for packaging of various products such as coffee, crackers, etc. Technical films for automatic or semi-automatic packaging of solid products (grains, powdered, etc.), liquids (milk, yogurt, etc.), and frozen foods (poultry, beef cuts, seafood, ice, etc.).

Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.

Information provided by Dax Resinas

Available Properties
  • Density
  • Thickness
  • Melt Index of Compound
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Secant Modulus, MD
  • Secant Modulus, TD
  • Coefficient of Friction
  • Elmendorf Tear Strength, MD
  • Elmendorf Tear Strength, TD
  • Dart Drop Test
  • Haze
  • Gloss
  • Processing Temperature
  • Feed Temperature
  • Adapter Temperature
  • Die Cooling Temperature
  • Blow-up Ratio (BUR)
  • Die Gap mm
  • Proportion LLDPE %
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。