DayGlo ZQ Pigments ZQ-18, Signal Green
Subcategory: Additive/Filler for Polymer
Key Words: Pigment; Colorant
Material Notes: DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have larger particle size to reduce dusting.Applications: - Polyethylene
- Polypropylene
- Polystyrene
- ABS
- Ionomer
- PA (Nylon)
- Polycarbonate
- Acrylic
- Rigid PVC
- Urethane