DENKA STYROL MW1 Polystyrene
Subcategory: Polystyrene; Thermoplastic
Material Notes: "DENKA SYTROL MW" is a well-balanced polystyrene (PS) resin, with a high tensile strength as well as good moldability. Overturning the traditional understanding that PS resin is "hard and brittle," this products applications have been expanded to include large packaging cases (and the like), advancing the world of PS resin, and becoming a synonym for ultra-strong PS.Applications - Recording media-related items like CD jewel cases, and videotape or audiocassette cases, etc.
- Refrigerator trays
- Pet cages
- Miscellaneous goods/toys
- Food packaging, etc.
| Available Properties |
- Density
- Melt Flow
- Spiral Flow
- Hardness, Rockwell M
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Charpy Impact, Notched
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Mold Temperature
- Injection Pressure
- Back Pressure
- Falling Weight Test, g/cm
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|