DENKA Transparent Resin TX Polymer (MS resin) TX-100S Methyl Methacrylate Styrene
Subcategory: Methacrylate; Thermoplastic
Material Notes: "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a good balance of transparency, strength and fluidity (methyl methacrylate butadiene styrene), "TE Series/CL Series," transparent ABS resins with excellent color attributes and tensile strength are available (among others).Applications TX is used for: - flat display substrates
- optical components
- miscellaneous goods.
TP/TH are used for:- food package sheeting as well as in manufacturing
- electronic equipment and components
- miscellaneous goods
TE/CL are for:- electronic equipment and components
- information equipment components
- AV equipment, etc.
| Available Properties |
- Density
- Specific Gravity
- Melt Flow
- Hardness, Rockwell M
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Charpy Impact, Notched
- Izod Impact Resistance
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Haze
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|