DENKA VINYKON M1600 PVC, M grade for hard injection molding
Subcategory: Vinyl; Thermoplastic
Material Notes: A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding, etc.
| Available Properties |
- Density
- Tensile Strength at Break
- Elongation at Break
- Penetration
- Izod Impact, Notched
- Vicat Softening Point
- Thermostability, min, JIS-K-6723
|
|
|
|