DENKA VINYKON W4050 PVC, W grade for equipment cords, for heat resistance
Subcategory: Vinyl; Thermoplastic
Material Notes: A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding, etc.
| Available Properties |
- Density
- Deformation
- Hardness, Shore A
- Tensile Strength at Break
- Elongation at Break
- 100% Modulus
- Volume Resistivity
- Minimum Service Temperature, Air
- Heating: Retention Rate of Elongation, %
- Heating: Retention Rate of Tensile Strength, %
- Oil Resistance: Retention of Tensile Strength, %
- Oil Resistance: Retention Rate of Elongation, %
- Thermostability, min, JIS-K-6723
|
|
|
|