DENKA REOMER G G3015 Thermoplastic Elastomer, For Extrusion

 

Subcategory: Elastomer, TPE; Thermoplastic

Material Notes:
Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive distortion, rebound elasticity, etc. compared to soft PVC, and excellent bending strength and ozone resistance compared to rubber

Applications

[Automotive components]

  • door moldings
  • weather-strips
  • glass run channels
  • side bumpers
  • gaskets
  • mud flaps
  • head rests
  • arm rests
  • steering wheels
  • trim
  • shift bar boots
  • pedal pads
[Construction material, manufacturing article home electric, appliance components]
  • gaskets
  • airtight materials
  • container packing
  • packing for vacuum cleaners
  • hoses
  • tubes
[For electric wire]
  • appliance cords
  • cabtire

Available Properties
  • Density
  • Evaporation Loss
  • Hardness, Shore A
  • Tensile Strength at Break
  • Elongation at Break
  • 100% Modulus
  • Resilience
  • Minimum Service Temperature, Air
  • Heating: Retention Rate of Elongation, %
  • Heating: Retention Rate of Tensile Strength, %
  • Oil Resistance: Retention of Tensile Strength, %
  • Oil Resistance: Retention Rate of Elongation, %
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。