DIAB Klegecell® R 130 Rigid, Closed Cell PVC Foam Core Material
Subcategory: Vinyl; Composite Core Material
Material Notes: Klegecell R is a PVC based, rigid, closed-cell foam with a tri-dimensional grid structure, which provides high thermal stability and structural integrity. As a structural core, Klegecell R is used in conjunction with high strength facings to produce lightweight, yet exceptionally stiff composite structures. Klegecell is widely used and found in pleasure crafts, tanks, high performance boats, vehicles, and many other high-strength, low-weight applications. Information provided by DIAB, Inc.
| Available Properties |
- Density
- Water Vapor Transmission
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Compressive Strength
- Compressive Modulus
- Poissons Ratio
- Shear Modulus
- Shear Strength
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Insulation R Value
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Processing Temperature
- Water Absorbtion
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|