Network Polymers, Inc. MS 130HF Styrene Methyl Methacrylate Terpolymer
Subcategory: Polystyrene; Acrylic; Thermoplastic
Material Notes: Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|