Network Polymers, Inc. NPP 20-3401 C/AS
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description: Random Copolymer Polypropylene, Clarified, with AntistatInformation provided by Network Polymers Inc.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|