Network Polymers, Inc. F20-52 Kepital®
Subcategory: Acetal; Thermoplastic
Material Notes: Description: Natural Acetal Copolymer, Weather Resistance GradeInformation provided by Network Polymers Inc.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell M
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Poissons Ratio
- Shear Strength
- Coefficient of Friction
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dissipation Factor
- Arc Resistance
- CTE, linear 68°F
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|