Dielectric Polymers NT-2802SW Functional Splice Tape
Subcategory: Silicone; Adhesive; Polyester, TS; Thermoset; Tape
Material Notes: Crosslinked silicone adhesive with silicone easy release coated polyester film backing. Features: - Chemical resistant
- Temperature resistant
- Good conformability
Applications: Splicing of roll label stock and substrates to be coated with a pressure sensitive adhesive. The silicone easy release coating on the back side of the PET creates a functional splice, making it ideal for sequential label applications. Also used to cover idlers and other in-process rolls that come in contact with pressure sensitive adhesives. Information provided by Dielectric Polymers.
| Available Properties |
- Thickness
- Elongation at Break
- Peel Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
- Shear Adhesive Failure Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|