Dielectric Polymers NT-2802 Ultra Tack Tape
Subcategory: Silicone; Adhesive; Polyester, TS; Thermoset; Tape
Material Notes: Crosslinked silicone adhesive with polyester film backing. Features: - Chemical resistant
- Temperature resistant
- Good conformability
Applications: Splicing of silicone coated paper and film at zero wet out time. For applications where instant adhesion is critical. Information provided by Dielectric Polymers.
| Available Properties |
- Thickness
- Elongation at Break
- Peel Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
- Shear Adhesive Failure Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|