Dielectric Polymers NT-988 High Tack Laminating Adhesive
Subcategory: Silicone; Adhesive; Acrylic; Thermoset
Material Notes: Acrylic copolymer adhesive with silicone treated release paper liner. Features: - Excellent adhesion to low surface energy substrates
- Compatible with most printing inks
Applications: Mounting a wide variety of substrates where quick adhesion is critical including coarse, uneven materials, low surface energy films and reverse printed materials. Information provided by Dielectric Polymers.
| Available Properties |
- Thickness
- Peel Strength
- Maximum Service Temperature, Air
- Shear Adhesive Failure Temperature
|
|
|
|