Dielectric Polymers NT-141PLT Double Liner Tape
Subcategory: Polyethylene; Adhesive; Acrylic; Thermoset; Tape
Material Notes: Acrylic adhesive with moisture stable PE coated kraft base release and high density PE interliner. Features: - Clear releases liner allows easy inspection of back lighted panels
- Plasticizer migration resistant
- Chemical resistant
Applications: Mounting nameplates, graphic panels and decorative trim. Bonding a wide variety of substrates. Information provided by Dielectric Polymers.
| Available Properties |
- Thickness
- Peel Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Shear Adhesive Failure Temperature
|
|
|
|
| Property Data |