Dielectric Polymers TRANS-SIL® NT-1001 Silicone Transfer Adhesive
Subcategory: Silicone; Adhesive; Polyester, TS; Thermoset
Material Notes: Crosslinked silicone adhesive with 2 polyester film release liners. Features: - Resistant to extreme temperatures
- High bond strength
- Chemical resistant
Applications: High performance bonding and other applications involving harsh environments. Bonds well to silicone foam, metals and most plastics including low surface energy substrates. Information provided by Dielectric Polymers.
| Available Properties |
- Thickness
- Peel Strength
- Dielectric Breakdown
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Shear Adhesive Failure Temperature
|
|
|
|