Domo Domamid® 24 T Polyamide 6
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: DOMAMID® 24 T are a low viscous Polyamide 6 pellets produced from Caprolactam by polymerization. Domamid T products are special textile grades with a high uniformity of relative viscosity and Amino-end groups.Applications: Textile yarn extrusionCompounding Injection moulding Information provided by Domo