Domo Domamid® 2403 T-HS Polyamide 6
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: DOMAMID® 2403 T-HS are a low-viscous Polyamide 6 pellets produced from Caprolactam by polymerization. Domamid®-T-products are special textile grades with a high uniformity of relative viscosity and Amino-end groups. Domamid®-HS-products are high stabilized grades for production of textile yarns in high speed spinning processes.Applications: Production of high quality textile yarns (improved evenness of dye take up and melt stability) Information provided by Domo
| Available Properties |
- Density
- Volatiles
- Apparent Bulk Density
- Viscosity Measurement
- Melting Point
- Moisture Content
- Chip Number
- Titanium Dioxide
|
|
|
|