Dow BETAMATE™ 5103-2 Epoxy
Subcategory: Epoxy; Thermoset
Material Notes: BETAMATE™ 5103-2 is a one component heat curing Epoxy paste adhesive. The material is readily pumped at ambient temperatures. It shows excellent adhesion to automotive steel, including coated steels, is resistant to degradation and to substrate corrosion on environmental aging. The product is precurabel to induction and compatible with electro-coat paint process.Information provided by Dow
| Available Properties |
- Density
- Solids Content
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Shear Strength
- Peel Strength
- Flash Point
- Extrusion Rate
- Cure Time
|
|
|
|