Dow BETAMATE™ 7000/7050 L Epoxy
Subcategory: Epoxy; Thermoset
Material Notes: Two component room temperature fast curing polyurethane structural adhesive with high elastic modulus.Information provided by Dow
| Available Properties |
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Shear Strength
- Cure Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|