Dow Buna® cis 132 High-cis polybutadiene rubber (nickel catalyzed) for tires and rubber articles

 

Material Notes:
Buna® cis 132 - Schkopau is a stereospecific polybutadiene with high cis-1,4 content. It is manufactured by a solution process using an organo-metallic catalyst which produces a consistent light colored polymer with low ash content. It contains a non-staining stabilizer. Buna® cis 132 is widely used in the tire industry but also in the manufacture of conveyor belts and other rubber articles which are exposed to high stress. It offers good abrasion resistance, high resilience, low hysteresis, and low glass transition point which results in better low temperature performance.

Buna® cis 132 offers excellent processability and may be blended with natural rubber and styrene butadiene (SBR), isoprene (IR), nitrile (NBR), or polychloroprene (CR) synthetic rubbers. The non-staining stabilizer allows manufacture of colored rubber articles also when compounded with selected thermoplastics. It is supplied in bales weighing 25 kg. Bales are wrapped in 50 micron PE film.

Information provided by Dow

Available Properties
  • Viscosity Measurement
  • Mooney Viscosity
  • Ash
  • Collected Volatile Condensable Material
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Shelf Life
  • Accelerator (TBBS) wt%
  • Carbon Black wt%
  • Cis-1,4 Content %
  • Stearic Acid wt%
  • Sulfur content, %
  • Zinc Oxide wt%
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。