Dow CYCLOTENE™ 4026-46 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
Material Notes: CYCLOTENE™ 4026-46 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Information provided by Dow
| Available Properties |
- Viscosity Measurement
- Thickness
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Poissons Ratio
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Thermal Conductivity
- Transformation Temperature, Tg
- Shrinkage
- Leakage Current A/cm²
- Stress on Si MPa, Min
|
|
|
|