Dow DAF 780 Carpet Underlayment Adhesion Film
Subcategory: Adhesive; Thermoset; Polymer
Material Notes: DAF 780 is a low melt point, coextruded film used to improve slip characteristics of polyurethane foam for carpet installation or other applications.Information provided by Dow
| Available Properties |
- Thickness
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|