Dow STYRON™ A-TECH™ 1115 High-Impact Polystyrene Resin
Subcategory: Polystyrene; Thermoplastic
Material Notes: STYRON™ A-TECH™ 1115 advanced technology polystyrene resin is a high gloss, high-impact resin for injection molding and extrusion thermoforming applications.
Main Characteristics - Easy Processing
- High Gloss
- High Impact
- Consistent Color-ability
- Complies with U.S. FDA 21 CFR 177.1640
Applications - Custom High Gloss Extruded Sheet
- Opaque Injection Molded Parts
- Refrigeration Accessories
- Small Appliances
- Electric Lawn and Garden Equipment
- Toys
- Remote Controls
Information provided by Dow
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Gardner Impact @ 23°C
- Izod Impact, Notched
- CTE, linear 68°F
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|