Dow TONE™ 0310 Polyol
Subcategory: Polyurethane, TS; Thermoset; Polymer
Material Notes: TONE™ 0310 polyol is a very low melting tri-functional liquid polyol for use in polyurethane elastomers, coatings, adhesives and soft foams.Information provided by Dow
| Available Properties |
- Specific Gravity
- Viscosity Measurement
- Molecular Weight
- Maximum Moisture Content
- Total Acid Number
- Melting Point
- Hydroxyl Number mg KOH/g
|
|
|
|
| Property Data |