Dow SE SLR-4610 H Solution polymerized Styrene Butadiene Rubber (S-SBR)
Subcategory: Styrene-Butadiene; Elastomer, TS; Thermoset
Material Notes: SE SLR-4610 H is manufactured by anionic solution polymerization using lithium initiator and is extended with 37.5 parts of aromatic oil in relation to solid rubber. It is a product with medium styrene and high vinyl content. The product is partially Sn-coupled and non-staining stabilized. SE SLR-4610 H is widely used in the tire industry for the manufacture of high performance tires providing excellent balance between rolling resistance, wet grip, and abrasion resistance. It is supplied in bales weighing 25 kg. Bales are wrapped in 50 micron PE film. At mixing temperatures above 110°C, the rubber can be processed with the packaging film. Information provided by Dow
| Available Properties |
- Viscosity Measurement
- Mooney Viscosity
- Vinyl Acetate Content
- Collected Volatile Condensable Material
- Storage Temperature
- Styrene Content
- Hardness, Shore A
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Rebound
- Vicat Softening Point
- Glass Temperature
- Shelf Life
- Accelerator (TBBS) wt%
- Carbon Black wt%
- Stearic Acid wt%
- Sulfur content, %
- Total Extractables %
- Zinc Oxide wt%
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|