Dow UVI-6976 Photoinitiator
Subcategory: Epoxy; Thermoset
Material Notes: UVI-6976 is a cationic photoinitiator containing a mixture of triarylsulfonium hexafluoroantimonate salts in propylene carbonate. UVI-6976 photoinitiator is used to UV-cure CYRACURE™ cycloaliphatic epoxide resins, vinyl ethers and other cationically curing materials.Information provided by Dow
| Available Properties |
- Specific Gravity
- Maximum Moisture Content
- Gardner Color Number
- Hydroxyl Number mg KOH/g
|
|
|
|