Dow Automotive BETAGUARD™ 64362 Expandable body shop sealer
Subcategory: Thermoset; Polymer; Adhesives, Sealants, and Coatings
Material Notes: Betaguard 64362 is a PVC base sealant. Its primary function is to seal interior and exterior seams. It has excellent paintability with OEM paint.Information provided by Dow
| Available Properties |
- Density
- Volatile Organic Compounds (VOC) Content
- Viscosity Measurement
- Tensile Strength, Ultimate
- Elongation at Break
- Cure Time
|
|
|
|