Dow Automotive INSPIRE™ TF1500 ESU Polypropylene
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Talc filled, high impact PP compound. INSPIRE™ TF1500 ESU has been developed for aesthetic automotive applications, with good scratch resistance and UV light stabilization.Information provided by Dow
| Available Properties |
- Density
- Filler Content
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched (ISO)
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Shrinkage
|
|
|
|
| Property Data |